Ngenxa yokuba iinzuzo zewelding laser, njengokuchaneka okuphezulu, ukusebenza kakuhle okuphezulu, ukusebenza okulula kunye nokulula, kusetyenziswe kumashishini amaninzi nangaphezulu, kodwa kuya kubakho iziphene kwinkqubo ye-welding, ekhokelela kwi-welding engafezekanga, indlela yokunciphisa okanye ukuphepha ukuvela kwezi ngxaki, ukubona isisombululo esishwankathelwa ngabavelisi bezixhobo zokuwelda i-laser.
Izisombululo zokuqhekeka:
Iintanda eziveliswe kwi-welding yomatshini we-laser welding ubukhulu becala ziintanda ezishushu, ezifana neentanda ze-crystallization, iintanda ze-liquefaction, njl., Isizathu sale meko kukuba i-weld ivelisa amandla amakhulu okunciphisa phambi kokuqina okupheleleyo, kuba oku kuqhekeza kunokuba ukunciphisa okanye ukupheliswa ngokuzalisa ucingo, ukufudumala kunye namanye amanyathelo.
Izisombululo kwimingxuma yomoya:
Uninzi lwe-welding luqhelekile kwingxaki ye-porosity, oku kungenxa yokuba i-laser welding pool inzulu kwaye imxinwa, isantya sokupholisa sikhawuleza kakhulu, kwaye irhasi eveliswa kwidama elinyibilikisiweyo lolwelo ayinaxesha laneleyo lokubaleka, okukhokelela ekwenziweni. ye porosity.Nangona kunjalo, i-laser welding iphola ngokukhawuleza, kwaye i-porosity eveliswayo ihlala incinci kunaleyo ye-welding yendabuko yokudibanisa.Umphezulu we-workpiece unokucocwa phambi kwe-welding ukunciphisa ukuthambekela kwee-pores, kwaye ulwalathiso lokuvuthela luya kuchaphazela ukubunjwa kwee-pores.
Isisombululo sokutshiza:
I-splash eveliswe yi-laser welding ayiyi kungcolisa kwaye yonakalise i-lens kuphela, kodwa iya kuchaphazela kakhulu umgangatho we-weld.Isizukulwana se-spatter sinxulumene ngokuthe ngqo noxinaniso lwamandla, kwaye ukuncipha okufanelekileyo kwamandla we-welding kunokunciphisa i-spatter.Ukuba ukungena akwanelanga, isantya se-welding sinokuncitshiswa.
Izisombululo zokuluma emaphethelweni:
Ukuba isantya welding ikhawuleza kakhulu kwi welding, isinyithi elulwelo emva umngxuma encinane elatha embindini weld akanalo ixesha lokuphinda usasaze, kwaye ukuqina macala omabini weld kuya kwenza edge bite.I-gap yendibano edibeneyo inkulu kakhulu, isinyithi esinyibilikayo se-caulk siyancitshiswa, kwaye umphetho ulula ukulunywa.Ekupheleni kwe-laser welding, ukuba ixesha lokuhla kwamandla likhawuleza kakhulu, umngxuma omncinci kulula ukuwa, okubangela ukuluma kwendawo, amandla okulawula kunye nokulinganisa isantya kunokuba sisisombululo esihle kwisizukulwana sokuluma.
Isisombululo sokuwa ezintlanu:
Ukuba isantya welding uyacotha, ichibi otyhidiweyo likhulu kwaye banzi, isixa esinyibilikisiweyo iyanda, kunye noxinzelelo umphezulu kunzima ukugcina metal ulwelo enzima, iziko weld uya kutshona, ukwenza ukudilika kunye nemingxuma.Ngeli xesha, kuyimfuneko ukunciphisa ngokufanelekileyo ubuninzi bamandla ukuze ugweme ukuwa kwedama elityhidiweyo.
Izizathu zeengxaki ze-laser welding ezahlukeneyo zahlukile, kwaye kufuneka siqale sifumane izizathu zohlalutyo lwengxaki ukuze sifumane unyango oluhambelanayo.Okunye malunga nezisombululo ze-welding eziqhelekileyo zomatshini we-laser welding wamkelekile ukutyelela iwebhusayithi yethu ukuze uqonde.Inkampani yethu ibonelela ngazo zonke iintlobo zomatshini wokuwelda we-laser,umatshini wokusika we-laser, izixhobo zomatshini wokumakisha laser, iimodeli ezipheleleyo, umgangatho othembekileyo, inkonzo egqibeleleyo, ukukhathazeka simahla emva kokuthengisa.
Ixesha lokuposa: Aug-04-2023